RavenMatte H550 Black mug

Serial Number: AJ24026
Run/Test Number: P6816
Technique: Thrown, engobed, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - GR10-C
Glaze Outside - GR10-C
Engobe - L3954N
Clay Body - H550
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 97 mm (3.8 in)
Depth at rim (including handle) - 126 mm (5.0 in)
Height - 116 mm (4.6 in)
Weight - 370 grams (13.0 oz)

Price:$35.00 (Not for sale, pieces being held for demo purposes)


PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy