Copper blue-green Polar Ice translucent porcelain mug

Serial Number: AJ24160
Run/Test Number: P6746
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G3806C
Clay Body - Polar Ice
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 80 mm (3.1 in)
Depth at rim (including handle) - 114 mm (4.5 in)
Height - 108 mm (4.3 in)
Weight - 284 grams (10.0 oz)