Serial Number: AJ24132
Run/Test Number: L4062A
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, bisque fired, dip glazed
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G2571A
Glaze Outside - G2571A
Engobe - L3954N
Clay Body - H550
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 97 mm (3.8 in)
Depth at rim (including handle) - 130 mm (5.1 in)
Height - 126 mm (5.0 in)
Weight - 420 grams (14.8 oz)
Price:$36.00 (Not for sale, pieces being held for demo purposes)