Serial Number: AJ24376
Run/Test Number: L4484
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside. I process raw clay lumps manually by slaking, slurry-up, sieving and dewatering on a plaster table.
Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - GA6-B
Glaze Outside - G2934Y Red
Clay Body - L4484 MNP
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 88 mm (3.5 in)
Depth at rim (including handle) - 119 mm (4.7 in)
Height - 0 mm (0.0 in)
Weight - 320 grams (11.3 oz)
Price:$50.00 (Not for sale, pieces being held for demo purposes)