Floating-blue stoneware mug

Serial Number: AJ24425
Run/Test Number: P7024
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G3914A
Glaze Outside - GR6-M
Clay Body - M340
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 91 mm (3.6 in)
Depth at rim (including handle) - 122 mm (4.8 in)
Height - 104 mm (4.1 in)
Weight - 358 grams (12.6 oz)

Price:$35.00 (Not for sale, pieces being held for demo purposes)