Oct 22, 2026: We are working on protecting our servers against the PHP2Shell vulnerability recently discovered. Servers were upgraded ahead of schedule on Oct 21. This could cause some issues. Please contact us if you encounter any.
![]() | ![]() | ![]() | ![]() |
Serial Number: AJ24022
Run/Test Number: L3924C
Technique: Thrown, leather-hard under-glaze decorated, incised, 1650F bisque fired, dip-glazed
Firing Schedule - C04PLTP
Temperature - Cone 03
Glaze Inside - G2931K
Glaze Outside - G2931K
Clay Body - L3924C
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 83 mm (3.3 in)
Depth at rim (including handle) - 113 mm (4.4 in)
Height - 119 mm (4.7 in)
Weight - 312 grams (11.0 oz)
Price:$40.00 (Not for sale, pieces being held for demo purposes)