Serial Number: AJ50018
Run/Test Number: L4686A
Technique: Thrown, incised, dip-glazed
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G1947U
Glaze Outside - G2880A Tenmoku
Clay Body - L4686A
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 95 mm (3.7 in)
Depth at rim (including handle) - 125 mm (4.9 in)
Height - 115 mm (4.5 in)
Weight - 360 grams (12.7 oz)
Not for sale