Folded Polar Ice porcelain Sunshine mug

Serial Number: AJ24128
Run/Test Number: P6803
Technique: Hand-assembled, pour-glazed inside, waxed, liner-glazed inside, dip-glazed outside

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G2934Y Yellow
Clay Body - Polar Ice
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 95 mm (3.7 in)
Depth at rim (including handle) - 124 mm (4.9 in)
Height - 98 mm (3.9 in)
Weight - 286 grams (10.1 oz)

Price:$35.00 (Not for sale, pieces being held for demo purposes)