Green and black porcelain mug

Serial Number: AJ24312
Run/Test Number: P6928
Technique: Thrown, liner-glazed inside, dip-glazed outside

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G3914A
Glaze Outside - G2934Y 6213
Clay Body - M370
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 99 mm (3.9 in)
Depth at rim (including handle) - 126 mm (5.0 in)
Height - 111 mm (4.4 in)
Weight - 352 grams (12.4 oz)