Blue Polar Ice porcelain mug

Serial Number: AH24300
Run/Test Number: P6923
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G2934Y Blue
Clay Body - Polar Ice
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 94 mm (3.7 in)
Depth at rim (including handle) - 125 mm (4.9 in)
Height - 115 mm (4.5 in)
Weight - 348 grams (12.3 oz)