Satin black MNS stoneware mug

Serial Number: AJ240190
Run/Test Number: L4208C
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - GA6-B
Glaze Outside - G2934Y Black
Clay Body - L4208C MNS
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 92 mm (3.6 in)
Depth at rim (including handle) - 121 mm (4.8 in)
Height - 102 mm (4.0 in)
Weight - 306 grams (10.8 oz)

Price:$40.00 (Not for sale, pieces being held for demo purposes)


PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy