Serial Number: AJ24103
Run/Test Number: P6622
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, bisque fired, dip glazed
Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - GA6-C
Glaze Outside - GA6-C
Engobe - L3954B
Clay Body - M340
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 107 mm (4.2 in)
Depth at rim (including handle) - 138 mm (5.4 in)
Height - 109 mm (4.3 in)
Weight - 526 grams (18.5 oz)
Reluctantly Sold (to Désire at my dental office)