Floating-blue stoneware mug

Serial Number: AJ24318
Run/Test Number: P6904
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G3914A
Glaze Outside - GA6-B
Engobe - L3954B
Clay Body - M340
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 101 mm (4.0 in)
Depth at rim (including handle) - 132 mm (5.2 in)
Height - 115 mm (4.5 in)
Weight - 446 grams (15.7 oz)

Price:$35.00 (Not for sale, pieces being held for demo purposes)


PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy