Serial Number: AJ24336
Run/Test Number: L4382A
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, bisque fired, dip glazed
Description: This H550 compatible clay body is made from Flintoft, Saskatchewan ball clay and Plainsman 3D.
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G2571F
Glaze Outside - G2571F blue MgO matte
Engobe - L3954N
Clay Body - H550 test
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 98 mm (3.9 in)
Depth at rim (including handle) - 130 mm (5.1 in)
Height - 106 mm (4.2 in)
Weight - 341 grams (12.0 oz)