Serial Number: AJ24351
Run/Test Number: P6767
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G2926B purple
Clay Body - Polar Ice
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 93 mm (3.7 in)
Depth at rim (including handle) - 127 mm (5.0 in)
Height - 111 mm (4.4 in)
Weight - 377 grams (13.3 oz)
Price:$40.00 (Not for sale, pieces being held for demo purposes)