Oatmeal glazed stoneware mug

Serial Number: AJ50050
Run/Test Number: L4761
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside. I process raw clay lumps manually by slaking, slurry-up, sieving and dewatering on a plaster table.

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - GA6-B
Glaze Outside - G3939E
Clay Body - Coffee Clay
Foot Style - Unglazed flat