Medalta 66 style bamboo mug

Serial Number: AJ24345
Run/Test Number: L4239
Technique: Jiggered, dip-glazed, cast handle

Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G2571A Bamboo
Glaze Outside - G2571A bamboo matte
Clay Body - H550 Casting
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 94 mm (3.7 in)
Depth at rim (including handle) - 122 mm (4.8 in)
Height - 110 mm (4.3 in)
Weight - 428 grams (15.1 oz)

Price:$35.00 (Not for sale, pieces being held for demo purposes)