Serial Number: AJ24077
Run/Test Number: P6823
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - L3500G+2Fe
Glaze Outside - GA6-C
Clay Body - M350
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 100 mm (3.9 in)
Depth at rim (including handle) - 129 mm (5.1 in)
Height - 116 mm (4.6 in)
Weight - 431 grams (15.2 oz)
Price:$35.00 (Not for sale, pieces being held for demo purposes)