Black silky matte MNS mug

Serial Number: AJ24314
Run/Test Number: L4208C
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - GA6-B
Glaze Outside - G2934Y Black
Clay Body - L4208C MNS
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 90 mm (3.5 in)
Depth at rim (including handle) - 120 mm (4.7 in)
Height - 107 mm (4.2 in)
Weight - 334 grams (11.8 oz)