Black Polar Ice porcelain mug

Serial Number: AJ24401
Run/Test Number: P6923
Technique: Thrown, incised, dip-glazed

Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G3914A
Glaze Outside - G2934Y Black
Clay Body - Polar Ice
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 88 mm (3.5 in)
Depth at rim (including handle) - 123 mm (4.8 in)
Height - 115 mm (4.5 in)
Weight - 345 grams (12.2 oz)