Purple M340 mug

Run/Test Number: L3905J1C
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G2926B Purple
Clay Body - L3905J1C
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 101 mm (4.0 in)
Depth at rim (including handle) - 135 mm (5.3 in)
Height - 102 mm (4.0 in)
Weight - 375 grams (13.2 oz)