Serial Number: AJ24110
Run/Test Number: P6886
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G2926BL
Glaze Outside - G2934Y Red
Clay Body - M370
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 100 mm (3.9 in)
Depth at rim (including handle) - 133 mm (5.2 in)
Height - 120 mm (4.7 in)
Weight - 364 grams (12.8 oz)
Price:$50.00 (Not for sale, pieces being held for demo purposes)