Purple translucent Polar Ice porcelain mug

Serial Number: AJ24091
Run/Test Number: P6746
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G2926B Purple
Clay Body - Polar Ice
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 90 mm (3.5 in)
Depth at rim (including handle) - 119 mm (4.7 in)
Height - 105 mm (4.1 in)
Weight - 352 grams (12.4 oz)