Serial Number: AJ24137
Run/Test Number: L3924C
Technique: Thrown, leather-hard under-glaze decorated, incised, 1650F bisque fired, dip-glazed
Firing Schedule - C04PLTP
Temperature - Cone 03
Glaze Inside - G2931K
Glaze Outside - G2931K
Clay Body - L3924C
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 85 mm (3.3 in)
Depth at rim (including handle) - 118 mm (4.6 in)
Height - 122 mm (4.8 in)
Weight - 339 grams (11.9 oz)
Price:$40.00 (Not for sale, pieces being held for demo purposes)