Rutile blue buff MNS stoneware mug

Serial Number: AJ50014
Run/Test Number: L4484G
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside. I process raw clay lumps manually by slaking, slurry-up, sieving and dewatering on a plaster table.

Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - GA6-B
Glaze Outside - GA6-C
Clay Body - L4484G MNS
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 94 mm (3.7 in)
Depth at rim (including handle) - 122 mm (4.8 in)
Height - 100 mm (3.9 in)
Weight - 285 grams (10.0 oz)

Not for sale