Serial Number: AJ24334
Run/Test Number: P6881
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G1947U
Glaze Outside - G2571E gunmetal
Clay Body - P700
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 95 mm (3.7 in)
Depth at rim (including handle) - 128 mm (5.0 in)
Height - 128 mm (5.0 in)
Weight - 392 grams (13.8 oz)
Price:$30.00 (Not for sale, pieces being held for demo purposes)