Orange Polar Ice porcelain mug

Serial Number: AJ24042
Run/Test Number: P6746
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G2934Y Orange
Clay Body - Polar Ice
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 91 mm (3.6 in)
Depth at rim (including handle) - 121 mm (4.8 in)
Height - 123 mm (4.8 in)
Weight - 364 grams (12.8 oz)

Price:$45.00 (Not for sale, pieces being held for demo purposes)