Serial Number: AJ24009
Run/Test Number: P6819
Technique: Hand-rolled, embossed and assembled, liner-glazed inside, dip-glazed outside
Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - GA6-B
Glaze Outside - G2934Y Black
Clay Body - M340GS
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 98 mm (3.9 in)
Depth at rim (including handle) - 130 mm (5.1 in)
Height - 100 mm (3.9 in)
Weight - 309 grams (10.9 oz)
Price:$40.00 (Not for sale, pieces being held for demo purposes)