Serial Number: AJ50006
Run/Test Number: P6572
Technique: Thrown, incised, dip-glazed
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G1947U
Glaze Outside - G1947U
Clay Body - P700
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 89 mm (3.5 in)
Depth at rim (including handle) - 122 mm (4.8 in)
Height - 107 mm (4.2 in)
Weight - 309 grams (10.9 oz)
Not for sale