Serial Number: AJ24409
Run/Test Number: L4131
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - GR10-C
Glaze Outside - G2571A Bamboo
Engobe - L3954N
Clay Body - BMix
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 101 mm (4.0 in)
Depth at rim (including handle) - 134 mm (5.3 in)
Height - 118 mm (4.6 in)
Weight - 385 grams (13.6 oz)
Price:$45.00 (Not for sale, pieces being held for demo purposes)