Gun metal black incised stoneware mug

Serial Number: AJ24331
Run/Test Number: L4453C
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - GR10-C
Glaze Outside - G2571E gunmetal
Clay Body - H550
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 95 mm (3.7 in)
Depth at rim (including handle) - 98 mm (3.9 in)
Height - 127 mm (5.0 in)
Weight - 347 grams (12.2 oz)