Serial Number: AJ24383
Run/Test Number: P6570
Technique: Thrown, incised, dip-glazed
Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G2926B
Clay Body - Polar Ice
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 92 mm (3.6 in)
Depth at rim (including handle) - 125 mm (4.9 in)
Height - 117 mm (4.6 in)
Weight - 366 grams (12.9 oz)
Not for sale