Serial Number: AJ50019
Run/Test Number: L3905G1
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside. I process raw clay lumps manually by slaking, slurry-up, sieving and dewatering on a plaster table.
Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - GA6-C
Clay Body - L3905G1
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 95 mm (3.7 in)
Depth at rim (including handle) - 126 mm (5.0 in)
Height - 111 mm (4.4 in)
Weight - 368 grams (13.0 oz)
Not for sale