Floating-blue stoneware mug

Serial Number: AJ24361
Run/Test Number: L4471D
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - GR6-M
Glaze Outside - PLC6DS
Clay Body - M390 test
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 95 mm (3.7 in)
Depth at rim (including handle) - 128 mm (5.0 in)
Height - 109 mm (4.3 in)
Weight - 348 grams (12.3 oz)

Price:$35.00 (Not for sale, pieces being held for demo purposes)