Black matte/glossy porcelain mug

Serial Number: AJ24307
Run/Test Number: P6928
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G3914A
Glaze Outside - G2934Y Black
Clay Body - M370
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 101 mm (4.0 in)
Depth at rim (including handle) - 136 mm (5.4 in)
Height - 120 mm (4.7 in)
Weight - 408 grams (14.4 oz)

Price:$40.00 (Not for sale, pieces being held for demo purposes)