Translucent Polar Ice porcelain mug

Serial Number: AJ24049
Run/Test Number: P6803
Technique: Thrown, incised, dip-glazed

Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G2926B
Clay Body - Polar Ice
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 96 mm (3.8 in)
Depth at rim (including handle) - 131 mm (5.2 in)
Height - 108 mm (4.3 in)
Weight - 354 grams (12.5 oz)

Price:$35.00 (Not for sale, pieces being held for demo purposes)