Serial Number: AJ24366
Run/Test Number: P6967
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G2934Y red
Clay Body - Polar Ice
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 90 mm (3.5 in)
Depth at rim (including handle) - 121 mm (4.8 in)
Height - 110 mm (4.3 in)
Weight - 357 grams (12.6 oz)