Floating blue MNP black porcelain mug

Serial Number: AJ24436
Run/Test Number: L4484D
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside. I process raw clay lumps manually by slaking, slurry-up, sieving and dewatering on a plaster table.

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - GR6-M
Clay Body - L4484D MNP Black
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 96 mm (3.8 in)
Depth at rim (including handle) - 130 mm (5.1 in)
Height - 109 mm (4.3 in)
Weight - 322 grams (11.3 oz)