Orange Polar Ice porcelain mug

Serial Number: AJ24145
Run/Test Number: P6746
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G2826B
Glaze Outside - G2934Y Orange
Clay Body - Polar Ice
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 93 mm (3.7 in)
Depth at rim (including handle) - 123 mm (4.8 in)
Height - 124 mm (4.9 in)
Weight - 392 grams (13.8 oz)