Blue Crystal Matte H555 mug

Serial Number: AJ24135
Run/Test Number: P6842
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - GR10-C
Glaze Outside - G2571C
Clay Body - H555
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 93 mm (3.7 in)
Depth at rim (including handle) - 125 mm (4.9 in)
Height - 111 mm (4.4 in)
Weight - 336 grams (11.8 oz)