White glazed speckled stoneware mug

Serial Number: AJ50002
Run/Test Number: P7051
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G3926B
Glaze Outside - G2936B
Clay Body - M340S
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 107 mm (4.2 in)
Depth at rim (including handle) - 139 mm (5.5 in)
Height - 125 mm (4.9 in)
Weight - 404 grams (14.2 oz)