Serial Number: AJ24154
Run/Test Number: L3875C
Technique: Thrown, incised, dip-glazed
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G1947U
Glaze Outside - G1947U
Clay Body - Polar Ice
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 93 mm (3.7 in)
Depth at rim (including handle) - 126 mm (5.0 in)
Height - 112 mm (4.4 in)
Weight - 328 grams (11.6 oz)
Price:$35.00 (Not for sale, pieces being held for demo purposes)