Serial Number: AJ24108
Run/Test Number: P6923
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G2934Y Blue
Clay Body - Polar Ice
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 97 mm (3.8 in)
Depth at rim (including handle) - 128 mm (5.0 in)
Height - 108 mm (4.3 in)
Weight - 360 grams (12.7 oz)
Price:$45.00 (Not for sale, pieces being held for demo purposes)