Matte red mug

Serial Number: AJ24378
Run/Test Number: P6973
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G3914A
Glaze Outside - G2934Y Red
Clay Body - M370
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 99 mm (3.9 in)
Depth at rim (including handle) - 135 mm (5.3 in)
Height - 128 mm (5.0 in)
Weight - 406 grams (14.3 oz)

Price:$50.00 (Not for sale, pieces being held for demo purposes)