Serial Number: AJ24320
Run/Test Number: P6902
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - GR10-C
Glaze Outside - G2571B
Engobe - L3954N
Clay Body - H450
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 97 mm (3.8 in)
Depth at rim (including handle) - 127 mm (5.0 in)
Height - 115 mm (4.5 in)
Weight - 393 grams (13.9 oz)