White matte glazed reduction fired mug

Run/Test Number: H555
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G1947U
Glaze Outside - GR10-C
Clay Body - H555
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 94 mm (3.7 in)
Depth at rim (including handle) - 125 mm (4.9 in)
Height - 116 mm (4.6 in)
Weight - 429 grams (15.1 oz)