Serial Number: AJ24126
Run/Test Number: P6748
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G1947U
Glaze Outside - GA10-A
Clay Body - P600
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 95 mm (3.7 in)
Depth at rim (including handle) - 123 mm (4.8 in)
Height - 122 mm (4.8 in)
Weight - 341 grams (12.0 oz)
Price:$35.00 (Not for sale, pieces being held for demo purposes)
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
Buy me a coffee and we can talk