Serial Number: AJ24325
Run/Test Number: L4376A
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, bisque fired, dip glazed
Description: H550 compatible clay body made from Flintoft, SK ball clay.
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G2571F
Glaze Outside - G2571F
Engobe - L3954N
Clay Body - H550 Test
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 97 mm (3.8 in)
Depth at rim (including handle) - 127 mm (5.0 in)
Height - 101 mm (4.0 in)
Weight - 328 grams (11.6 oz)