Matte red mug

Serial Number: AJ50001
Run/Test Number: P7027
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G3914A
Glaze Outside - G2934Y Red
Clay Body - M370
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 92 mm (3.6 in)
Depth at rim (including handle) - 129 mm (5.1 in)
Height - 119 mm (4.7 in)
Weight - 366 grams (12.9 oz)