Blue Polar Ice porcelain mug

Serial Number: AJ24047
Run/Test Number: P6746
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G2934Y Blue
Clay Body - Polar Ice
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 97 mm (3.8 in)
Depth at rim (including handle) - 128 mm (5.0 in)
Height - 127 mm (5.0 in)
Weight - 387 grams (13.6 oz)

Price:$45.00 (Not for sale, pieces being held for demo purposes)


PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy